Newby question alert....
So I perform the saturation curves prior to a new job/parameters. Then from that day forward anytime we do that job running to the set parameters at the beginning of the job I perform a an arc height verification and then I perform another when the job is complete - even if that is 2 days later.
First question: Is this the right approach?
Second question: Is there a standardized Inspection form for this process? no sense in reinventing the wheel if their is a form someone has created for capturing this information already - to include prebow measurements and prebow comp.