They are not completely wrong. Heating a part relieves/neutralizes the stress, however Peening goes beyond that and congresses the surface layer. A compressed surface allows cyclic loading thus improving fatigue life.
Dave Barkley EI SPT Director, Peening Preceptor & Product Engineer