I came across a report that listed fatigue testing of steel that was peened with S170 size cast steel(HRC 65) and ceramic shot to an intensity of 10A. The hardness of the ceramic shot was comparable to the steel. The average fatigue failure was about 25% higher in the samples peened with cast steel shot. Any ideas on what could have contributed to such a drastic difference in fatigue testing results?