I just sent it to your email. The ceramic bead is 6-7 MOHS which is in the ballpark of 65HRC. The data doesnt follow any of the expected trends such as the bead size and the affect of the resulting surface finish on fatigue strength. This report was mentioned in other reports i saw online.