Fine Particle Shot Peening (FPSP) Technology
Author: Mitsubishi
Source: Mitsubishi
Doc ID: 2018011
Year of Publication: 2018
Abstract:
Fine particle shot peening (FPSP) technology
- Technology, features
Basic fatigue properties of A7075 by FPSP
- S/N data and residual stress compared with conventional shot peening (SP) technology
Fatigue properties of FPSP A7075 followed by BSAA BSAA: Boric Sulfuric Acid Anodize
- Influence of anodizing after FPSP and SP
- SEM observations of surface, cross section and fracture cross
section