Laboratory Fatigue Testing Of Gears
Author: Halgren, John and Wulpi, D.J.
Source: SAE Journal, Sept. 10-13, 1956, #808
Doc ID: 1956003
Year of Publication: 1956
Abstract:
This paper deals with endurance testing of spur gears in modified four-square gear testing machines, also referred to as special gear testing dynamometers, power circulating gear testing machines, and single-pair gear test machines.