Air Blast Power Units For Shot Peening Applications
Author: Hill, E. J.
Source: Conf Proc: ICSP-1, (p.115-120)
Doc ID: 1981005
Year of Publication: 1981
Abstract:
The features that may be incorporated in air blast power units designed for general impact treatment applications to provide the control and monitoring necessary to meet the specific requirements of shot peening are described. Pneumatic recovery and ventilation systems are discussed.
Descriptors: Shot peening; Dust control; Reclamation; Monitoring