Characteristiques Des Grenailles Utilisees Shot Peening
Author: Arnaud, P.
Source: Conf Proc: ICSP-1, (p.109-114)
Doc ID: 1981013
Year of Publication: 1981
Abstract:
Shot peening can improve the fatigue behavior of materials. Therefore, the characteristics have to be well defined and controlled. The main parameters which can be evaluated on shot materials are given, and their influence on both the quality and the cost of peening determined.
Descriptors: Shot peening; Granular materials-- Mechanical properties; Particle size; Carbon steels; Hardness