The Strength Of Shot Peened Parts, Design Calculations And Specifications
Author: Fuchs, H.O.
Source: Conf Proc: ICSP-1, (p.323-332)
Doc ID: 1981077
Year of Publication: 1981
Abstract:
This paper presents a method for predicting the fatigue strength of shot peened parts at any given fatigue life. The method considers the different criteria for crack initiation, arrest of small cracks, and change of the self-stress by yielding. Guides are given for choosing a good peening intensity and for specifying the desired result.
Descriptors: Shot peening; Fatigue strength; Self-stress; Bi-axial stress; Haigh diagrams; Fatigue strength prediction; Crack arrest; Yielding; Almen intensity.