Extending the Service Life of Railroad Traction Gears
Author: Yudin, D.L.
Source: Soviet Engrg. Research 1(2): 37-38
Doc ID: 1981099
Year of Publication: 1981
Abstract:
With the increasing loading intensity of railways, and train speed and mass, growing attention is being paid to the problem of raising the strength and durability of traction reduction gearing.