Controlled Shot Peening Reduces Or Eliminates Stress Corrosion Cracking
Author: Feld, P.G. and Gillespie, R.D.
Source: Conf Proc: ICSP-2, (p.121-125)
Doc ID: 1984008
Year of Publication: 1984
Abstract:
Controlled Shot Peening (CSP) is a cost effective technique to reduce and/or eliminate stress corrosion cracking (SCC) failures which cost industry millions of dollars. Cases are shown.
Descriptors: Shot peening; Stress corrosion