On The Relation Between Delamination Wear And Microcrack Propagation
Author: Jiawen, He
Source: Conf Proc: ICSP-2, (p.266-268)
Doc ID: 1984049
Year of Publication: 1984
Abstract:
Compressive residual stress induced in shot peening enlarges the low crack growth rate region, it reduces delamination wear rate.
Descriptors: Delamination wear; Residual stress; Shot peening; Microcrack growth