Peening By Water
Author: Salko, Djosic
Source: Conf Proc: ICSP-2, (p. 37-39)
Doc ID: 1984052
Year of Publication: 1984
Abstract:
Steel has been peened by high velocity water jets. Advantages over shot peening are assured complete coverage and a smooth surface. Induced stresses are less than by shot peening. Equipment is briefly described.
Descriptors: Peening; Water peening; Vibrating stress-relief