Use Of Industrial Robots To Increase Productivity Of Peening Operation
Author: Johnston, W.S.
Source: Conf Proc: ICSP-2, (p. 34-36)
Doc ID: 1984072
Year of Publication: 1984
Abstract:
The purpose of this paper is to discuss the various ways industrial robots can be applied to increase the productivity of peening operations. In addition to an increase in productivity an increase in accuracy and repeatability can be achieved by proper application of industrial robots.
Descriptors: Repeatability; Process control, Robot protection