Additional Shot Peening For Workshop
Author: Salko, Djosic
Source: Conf Proc: ICSP-3, (p.163-168)
Doc ID: 1987000
Year of Publication: 1987
Abstract:
In one normal size manufacturing shop for different types of springs, gears, wheels, car parts, shafts etc. necessary to have special room for shot peening. As indicated on the fig. 1. after collection some quantities on the transport chain going on the further workmanship - shot peening. Shot peening plant enables to get the improvement of mechanical properties of that items.