Analysis Of Some Particular Cases Of Shot-peening And Their Influence On Field Of Residual Stresses
Author: Barret, L. and Cailliau, J.
Source: Conf Proc: ICSP-3, (p.399-406)
Doc ID: 1987002
Year of Publication: 1987
Abstract:
The distribution and intensity of residual stresses due to shot-peening are dependent upon a lot of parameters; some of them are involved with the material characteristics, the other ones are relying upon the shot-peening process conditions.
Preexisting stresses on the surface of the part in the initial state
have no influence on final state after shot-peening; on the opposite stresses applied after shot-peening operation may alter for a large part the field of residual stresses.
A theoretical approach has been developed and is conformable to
experimental results.