Important Considerations For Utilizing Shot Peening As A Design Tool
Author: Simpson, R.S. and Garibay, R.P.
Source: Conf Proc: ICSP-3, (p. 71-78)
Doc ID: 1987042
Year of Publication: 1987
Abstract:
The purpose of this paper is to ennumerate important considerations involved in utilizing the shot peening process as part of the design strength of a workpiece. It should be noted that, due to the need for brevity, much of the details essential to implementing shot peening into design strength have gone unmentioned.