Criterion To Select Materials For Shot Peening And Rolling Hardening
Author: Xingzeng, Xinlong, ZhongXing, Jianzhon
Source: Conf Proc: ICSP-4, (p.219-226)
Doc ID: 1990018
Year of Publication: 1990
Abstract:
The effect of residual stress forming during sholling peening and rolling was discussed. In this paper, we proved that attenuation of residual compression stress was relating to the compression yield limit +_(s).(c) and +_(s).(t) of materials, and pressent that if effect of surface deformation hardening is judged by fatigue strength change rate Delta +_(h)/+_(h), +_(b)(o)/+_(s)(c) may be regarding as a criterion. The larger +_(b)(o)/+_(s)(c) is, the better the surface hardening effect upon the materials is. So it is convenient to select materials for shot-peening and rolling hardening by the date of static compression behaviour of materials, which is practically valuable.
Descriptors: Deformation hardening; Attenuation of residual stress