Vibratory Burnishing Of External Cylindrical Surfaces
Author: Barski, T. and Gajek, M.
Source: Conf Proc: ICSP-4, (p.119-126)
Doc ID: 1990096
Year of Publication: 1990
Abstract:
The paper presents a prototype structural solution of a stand for vibratory burnishing of external cylindrical surface. It also discusses the influence of technological parameters of the treatment on surface roughness and dimensional accuracy of an object made of the constructional steel 45/Polish Standard/. The experiment was carried out with an application of the rotatable design type two/2(3)-type/and the obtained result has a form of a second degree polynominal