Application of Statistically Capable Shot Peening to Automotive Component Design
Author: Adam Vahratian, Robert Garibay
Source: Conf Proc: ICSP-5, (p. 99-110)
Doc ID: 1993054
Year of Publication: 1993
Abstract:
Today's workd automotive business climate is demanding more cost effective, higher strength/weight designs than ever before. Engineering coverage factors are shrinking and at the same time, designs are becoming more robust. Consequently, manufactureing processes without a quantified benefit/cost ratio are being descarded. Those processes that are utilized are required to statistacially demonstrate acceptable product performance.