Solution of Mechanica and Control Problems by Dynamic Condensation Method
Author: Kamen Ishtev and Philip Philipov
Source: Conf Proc: ICSP-5, (p. 28-33)
Doc ID: 1993058
Year of Publication: 1993
Abstract:
The paper discusses dynamic condensation method application for solving optimization and control problems in shot peening processes. Second order matrix differential equation is used to treating object modelling. It is assumed that only some degrees of freedom are sigmificant. All other degrees of freedom are eliminated by the dynamic condensation method. As a result the transfer function os obtained. It gives the possibility of analyzing a shot peening process and of input impact optimization.
| Download PDF |
|---|