Quality Control of Shot Media by Sieve Analysis
Author: Per Bohn
Source: Conf Proc: ICSP-5, (p. 65-72)
Doc ID: 1993062
Year of Publication: 1993
Abstract:
Concerning shot peen processing, the governing factors to ensure high quality results are more than steering of process and capabilities of equipment. The quality of shot media, be it manufactured from glass, steel, ceramic or any other materials, is vital in ensuring satisfactory process results.