Effects of Shot Peening and Heat Treatment on Endurance Limits of Austempered Ductile Cast Iron Gears
Author: S.Ezoe, M.Hashimoto, I.Asano, Y.Tanno
Source: Conf Proc: ICSP-6, (p. 14-23)
Doc ID: 1996047
Year of Publication: 1996
Abstract:
ADI materials are going to be applied to transmission gears. Endurance tests of the ADI gears were carried out to discuss summarily the effects of shot peening and heat treatment on the endurance limits of bending strength as well as surface durability. It is clarified that the shot peened ADI gears are suitable to gear materials due to the increase of the endurance limits, although those gears have rough surface. At the same time, special precautions are required in utilizing the ADI with a low hardness of base material and in using of oil with no EP additives as the endurance limits are restricted by surface durability.
| Download PDF |
|---|