Relaxation of Residual Stress Distribution Produced by Shot Peening Under Fatigue Test
Author: Kisuke Iida, Kazunori Taniguchi
Source: Conf Proc: ICSP-6, (p.397-402)
Doc ID: 1996085
Year of Publication: 1996
Abstract:
Residual stress distribution produced by shot peening was decreased in early time under fatigue test of plate bending method. shot peening was performed by steel shot intensity 0.15A-0.74A to annealed medium carbon steel specimens. Residual stress was measured by x-ray window process. The distributions of residual stress are all C type, which has the maximum stress at peened surface. Relaxation of residual stress distribution appeared exceedingly by small stress amplitude under fatigue test.