Peening Media (AWCH) Conditioned Carbon Steel Cut Wire Shot, High Hardness (55 to 62Hrc) AMS 2431/8

Author:  SAE
Source:  SAE: AMS 2431/8, REV 09/01/1996
Doc ID:  1996101
Year of Publication:  1996
Abstract:  
The complete requirements for procuring the product shall cinsist of this document and the latest issue of the basic specification AMS 2431