Test Strip, Holder and Gage for Shot Peening

Author:  SAE
Source:  SAE: J 442 Rev May 1997
Doc ID:  1997041
Year of Publication:  1997
Abstract:  
This SAE Standard defines requirements for equipmen/supplies to be used in measuring shot peening intensity. Guidelines for the use of these articles (test strip, holding fixture and gage) are also included.