Exfoliation Corrosion Located by Search Peening
Author: W Wubbenhorst
Source: Conf Proc: ICSP-7 (pg 209-215)
Doc ID: 1999032
Year of Publication: 1999
Abstract:
Exfoliation Corrosion, a more severe form of Intergranular Corrosion, occurs along aluminium grain boundaries which in sheet and plate are oriented parallel to the surface of the material, due to the rolling process. It is characterized by delamination of thin layers of the aluminium with white corrosion products between the layers.