Abstract:
This device is destinated to avoide difficulties with normal Shot Peening. This apparatus has two steel fabricated rolls: one is vertical and other horizontal in front of them are jets for normal Shot Peening. This way is combination of normal Shot Peening and impacting by rolling of two steel roller under angle 90