Ceramic Shot Enhancement of High Strength Steel Endurance Application to Springs and Gears
Author: F-X Abadie, L Barralier, S Fleury
Source: Conf Proc: ICSP-9 (pg 48-53)
Doc ID: 2005050
Year of Publication: 2005
Abstract:
ABSTRACT
This paper will briefly recall some previous research works on ceramic shot, expose latest complementary works, and show their translation into effective industrial applications for the improvement of fatigue behavious of springs and gears.