The Interest To Use Tungsten Carbide Balls With Stressonic Ultrasonic Shot-Peening Process: Application To Aero Engines Parts
Author: Jean-Michel Duchazeaubeneix, Sonats
Source: Conf Proc: ICSP-9 (pg 171-178)
Doc ID: 2005068
Year of Publication: 2005
Abstract:
ABSTRACT
Ultrasonic Shot Peening, Stressonic, developed by Sonats, is applied in industry since several years. In this paper we are presenting the principal of the Stressonic process. We are focusing also on the application for aero engines parts, especially blades, Blisks and disks and the interest to use Tungsten Carbides bearing balls for cost reduction and fatigue life improvement.