Shot Peening With Dry Ice
Author: E Uhlmann, M Krieg
Source: Conf Proc: ICSP-9 (pg 197-201)
Doc ID: 2005072
Year of Publication: 2005
Abstract:
ABSTRACT
Dry ice blasting is a compressed air process, which uses solid carbon dioxide CO2 at a temperature of -78.5