Peening Media (AWCH) Conditioned Carbon Steel Cut Wire Shot, High Hardness (55 to 62 Hrc) AMS 2431 8B

Author:  SAE
Source:  SAE: AMS 2431/8B 05/2007
Doc ID:  2007038
Year of Publication:  2007
Abstract:  
The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431.