Ricochet Peening
Author: P. Bailey, J. Champaigne, C. Long
Source: Conf Proc: ICSP-10 Tokyo, Japan 2008
Doc ID: 2008030
Year of Publication: 2008
Abstract:
Ricochet peening may be used in cases where it is impossible to obtain complete visual coverage by direct impact. AMS-S-13165 refers to this as reflected shot stream. This study illustrates the influence on the shot stream reflected angle and impact intensity as a function of material hardness.
KEY WORDS
Ricochet Peening, Reflected shot stream, Impact Angle, Ricochet Angle, Peening Coverage,