Improvement Of Fatigue Strength Of Light Metallic Materials By Cavitation Shotless Peening
Author: Y. Sekine, N. Miyamoto, H. Soyama
Source: Conf Proc: ICSP-10 Tokyo, Japan 2008
Doc ID: 2008054
Year of Publication: 2008
Abstract:
ABSTRACT
Cavitation normally causes severe damage in hydraulic machinery such as pumps, valves and so on. However, cavitation impact can be utilized to surface treatment to improve fatigue strength of metallic materials in the same way as shot peening. A peening method using cavitation impact was named as