Influence Of Shot Peening Treatment On The Fatigue Life Of Ti6ai4v Eli Biomedical Alloy
Author: S. Amin-Yavari, A.A. Ziaei-Moayed, H.R. Madaah-Hos
Source: Conf Proc: ICSP-10 Tokyo, Japan 2008
Doc ID: 2008096
Year of Publication: 2008
Abstract:
ABSTRACT
Fatigue lives of shot peened specimens have been evaluated by Rotating
| Download PDF |
|---|