Effect Of Laser Peening On Fatigue Prpoerties For Aircraft Structure Parts
Author: T. Adachi, H. Takehisa, M. Nakajima, Y. Sano
Source: Conf Proc: ICSP-10 Tokyo, Japan 2008
Doc ID: 2008107
Year of Publication: 2008
Abstract:
ABSTRACT
Laser peening is expected to improve fatigue properties more than shot peening, because it is possible to induce compressive residual stresses deeper than conventional treatments. In this study, we examined the applicability of laser peening to the aircraft through investigating the effects of laser peening on fatigue properties and the formability of aircraft parts.
KEYWORDS
Laser peening, Residual stress, Fatigue, Aluminum alloy, Helicopter