Influence Of Shot Peening On Fatigue Strength Of Friction Welded Joint
Author: H.Suzuki, M.Hasegawa
Source: Conf Proc: ICSP-10 Tokyo, Japan 2008
Doc ID: 2008125
Year of Publication: 2008
Abstract:
ABSTRACT
Effects of base metal hardness on improvement of fatigue strength by shot peening treatment are investigated using various carbon steels for machine construction. Furthermore