3D FE analysis of shotpeening process for simulation and research on shotpeening process parameters
Author: A. Manoucherifar and K. Rezvani
Source: Conf Proc 2011: ICSP-11 South Bend, IN USA (pgs. 67-74)
Doc ID: 2011011
Year of Publication: 2011
Abstract:
Abstract
The present research aims at describing a simplified 3D finite element dynamic and static analysis of shot impacting on metallic target plates to clarify and for better understanding of the effect of several key parameters such as shot velocity, shot size, incident angle, coefficient of friction and multiplicity of shot on compressive residual stress created by the shot-peening process. The finite element package ABAQUS 6.9 is used to simulate the procedure corresponding to the experimental operations. The geometry of the target plate is assumed to be a deformable plate with 2