Impact velocity and distribution in ultrasonic shot peening
Author: Badreddine, Micoulaut, Rouhaud, Retraint, Francois
Source: Conf Proc 2011: ICSP-11 South Bend, IN USA (pgs. 99-104)
Doc ID: 2011016
Year of Publication: 2011
Abstract:
Authors: Badreddine, Micoulaut, Rouhaud, Retraint, Francois, Remy
Abstract
We study the dynamic of shot during an ultrasonic shot peening process from two aspects. The first consists in running various calculations of spheres placed in a cylindrical chamber (radius 35 mm, height 40 mm) and propelled by a sonotrode (frequency 20 kHz, amplitude 25