Influence of Isothermal Annealing on Stress Relaxation of Shot Peened SiCw/Al Composite
Author: Huang, Jiang, Wang
Source: Conf Proc 2011: ICSP-11 South Bend, IN USA (pgs. 279-284)
Doc ID: 2011046
Year of Publication: 2011
Abstract:
Abstract: The residual stress relaxation of the shot peened layer on the SiCw/Al composite during isothermal annealing was investigated. The results showed that the residual stresses relaxed in the whole deformation layer especially when the annealing temperature was higher than 200