Influence of shot peening and superfinishing on gears as a repair tool of damaged faces of teeth generated by overheating whe
Author: Kritzler
Source: Conf Proc 2011: ICSP-11 South Bend, IN USA (pgs. 405-410)
Doc ID: 2011068
Year of Publication: 2011
Abstract:
Abstract
Hard finishing by grinding of case hardened gears is a common process in the gear industry with final roughness of the flank normally Ra= 0.2