Cast Shot and Grit Size Specifications for Peening and Cleaning

Author:  SAE
Source:  SAE: J444 SEP2012
Doc ID:  2012037
Year of Publication:  2012
Abstract:  
RATIONALE During the 2010 revision to this document a typo was made in Figure 1 for S-460 shot screening specification. The 5% max 1.7 mm sieve was changed to the 0% max and the 0% max 2.00 mm sieve became a non-specification sieve. These two errors have been corrected.