Abstract:
In the present work, an overview of modern mechanical surface treatments is given. The available technologies are classified by the type of tool-workpiece interaction.Selected treatments are presented in detail. Besides the description of each process technology, main focus is given to the characteristic resulting surface layer states. To this end, typical residual stress profiles and work hardening states as well as surface topographies are presented and compared
for those processes.
| Download PDF |
|---|