Mini-strips for Limited Access Peening Intensity Measurements
Author: J. Champaigne, J. Derda
Source: Conf Proc 2014: ICSP-12 Goslar, Germany (pgs.398-403)
Doc ID: 2014110
Year of Publication: 2014
Abstract:
The Almen strip as described in SAE J442 is widely used for measurement of peening intensity. There are some applications, however, where the strip size is too large for the intended measurement area. A sub-size strip can be used in those applications. This paper will dscribe the procedures for affixing and measuring this strip and how to correlate the Mini-strip arc height readings to the standard size Almen strip.
| Download PDF |
|---|