Development of Residual Stresses Induced by Deep Rolling at an Additive Structure
Author: E. Mueller
Source: ICSP14 Milan
Doc ID: 2022046
Year of Publication: 2022
Abstract:
This paper shows the residual stress distributions over the depth of a dice out of 1.2344
produced as an additive structure. Because of the layer structure (obtained by SLM) it gives
two interesting directions (along with the layer and perpendicular to the layer) to be
investigated concerning residual stresses. Next a deep rolling process was done. Deep rolling
gives different residual stress distribution. Perpendicular to the rolling track higher
compressive residual stress is induced in comparison along the track. Combined with the layer
structure of the dice, four different combinations are obtained that are investigated concerning
residual stresses.