Optimization of shot peening parameters on beta titanium alloy Ti10V-2Fe-3Al in order to improve fatigue behaviour
Author: M.R. Chinia, C. Didesb, T. Billot c, N. Guillemot d a, b IRT M2P, 4 rue Augustin Fresnel, 57070 Metz, France - maria-rita.chini@irt-m2p.fr, c SAFRAN LANDING SYSTEMS, 9 Rue Guynemer, 64400 Bidos, France - thomas.billot@safrangroup.com d AIRBUS HELICOPTERS,
Source: ICSP14 Milan
Doc ID: 2022062
Year of Publication: 2022
Abstract:
Shot peening is a mechanical surface treatment widely used in industry to improve the fatigue
properties of components. It appears that the parameters of this process must be adjusted to new
alloys and/or manufacturing techniques to reach even better fatigue properties. The purpose of
this study is to determine the optimal shot peening conditions for the beta titanium alloy Ti10V-
2Fe-3Al in order to optimize fatigue life, taking into account different machining conditions. This
development was carried out during CONDOR project.
Keywords: Shot peening, Fatigue, beta titanium, Ti 10V-2Fe-3Al, fractography, surface
roughness
| Download PDF |
|---|