Development of a peening device with a handheld laser on a collaborative robot
Author: Y. Sano1,2,3, Y. Mizuta1, S. Tamaki3, K. Yokofujita4, K. Masaki5, T. Hosokai1 and T. Taira2 1 SANKEN, Osaka University, Ibaraki, Japan 2 Institute for Molecular Science, National Institutes of National Sciences, Okazaki, Japan 3 LAcubed Co. Ltd., Yokohama
Source: ICSP14 Milan
Doc ID: 2022064
Year of Publication: 2022
Abstract:
A compact laser peening (LP) device has been developed for application to large structures
such as bridges in service. The device consists of a thumb-sized handheld laser mounted on
a collaborative robot, a power supply, a water circulation system, and a PC as a control unit.
Various materials such as aluminum alloys and high-strength steels were laser-peened by
using this device. Results of residual stress (RS) evaluation and fatigue experiments showed
that LP with this device significantly improved the RSs in the near-surface layer and fatigue
properties of materials.
Keywords Microchip laser, robotic arm, laser peening, residual stress, fatigue