New Electronic Peening Intensity Sensor: Comparison with Almen Arc Height Verification
Author: Sylvain A. Forgues 1, Brigitte Labelle1, Adel Alouani1, Ramzi Ben Moussa1 1Shockform Aeronautique Inc., Canada, engineering@shockform.com
Source: ICSP14 Milan
Doc ID: 2022089
Year of Publication: 2022
Abstract:
Keywords: Shot Peening, Electronic Intensity Sensor, Intensity Verification, Intensity
Histograms
Introduction
Almen strips are often used for peening intensity determination and verification. For intensity
verification, one must measure the pre-bow of the Almen strip, install the strip on the holder,
peen the strip for a period of time, remove the strip from the holder and measure the arc height
of the strip with a dedicated gage. For intensity determination, these steps must be repeated at
least four different times to generate a saturation curve. Intensity determination and verification
can account for 10% to 30% of machine usage.
| Download PDF |
|---|