New Electronic Peening Intensity Sensor for Pneumatic Needle Peening Repair Tools
Author: Adel Alouani1, Sylvain A. Forgues 1, Brigitte Labelle1, Ramzi Ben Moussa1 1Shockform Aeronautique Inc., Canada, engineering@shockform.com Keywords: Rotary Flapper Peening, Pneumatic Needle Peening, Portable Tools, Repair
Source: ICSP14 Milan
Doc ID: 2022090
Year of Publication: 2022
Abstract:
Keywords: Rotary Flapper Peening, Pneumatic Needle Peening, Portable Tools, Repair
Peening, Electronic Intensity Sensor
Introduction
Controlled pneumatic needle peening is often used after blending surface damage to rebuild the
residual compressive layer that is removed by the blend. Controlled pneumatic needle peening
can be used to peen surfaces on assembled aircraft with minimal dismantling and minimal risk of
Foreign Object Debris (FOD). This technique has the advantage of a small work-head to peen
difficult to reach areas while maintaining optimal stand-off distance at all times.