Evolution of the controlled shot peening process in the automotive field
Author: E. Morgano SILCO - Rivalta TO
Source: ICSP14 Milan
Doc ID: 2022105
Year of Publication: 2022
Abstract:
Introduction
The controlled shot peening process, on a mechanical component, represents the most robust
solution to increase its resistance to fatigue; moreover, since it is usually the last operation in the
production chain, it does not change the parameters of the previous operations, such as forging,
mechanical processing and surface hardening treatments.